主要研究成果 | 一、主要学术论文 [1] Tian, Linhai; Li, Xiaoying; Dong, Hanshan. Novel wear-resistant anti-bacterial stainless steel surfaces. Surface Engineering, 34(8), pp 577-587, 2018 [2] Qin, Lin; Yi, Hong; Kong, Fanyou; Ma, Hua; Guo, Lili; Tian, Linhai; Tang, Bin. Effect of plasma molybdenized buffer layer on adhesive properties of TiN film coated on Ti6Al4V alloy. Applied Surface Science, 403, pp 464-471, 2017-5-1 [3] 聂婷婷; 李小英; 田林海; 董汉山. AISI 316不锈钢表面银氮复合共渗及其磨损和抗菌性能. 中国表面工程, (04), pp 36-44, 2017-6-14 [4] Zhang, Linlin; Bao, Mingdong; Zheng, Qiang; Tian, Linhai; Du, Juan. Magnetocaloric effect in high Gd content Gd-Fe-Al based amorphous/nanocrystalline systems with enhanced Curie temperature and refrigeration capacity. AIP Advances, 6(3), pp 035220, 2016-3 [5] 张秀香; 李翔; 戴姣燕; 田林海; 徐金富. 45钢激光硼合金化工艺优化及性能研究. 兵器材料科学与工程, (01), pp 97-100, 2016-1-4 09:31 [6] Zhang, Xiangyu; Wang, Huizhen; Li, Jiangfang; He, Xiaojing; Hang, Ruiqiang; Huang, Xiaobo; Tian, Linhai; Tang, Bin. Corrosion behavior of Zn-incorporated antibacterial TiO2 porous coating on titanium. Ceramics International, 42(15), pp 17095-17100, 2016-11-15 [7] Yao Xiaohong; Xie Penghua; Sun Yonghua; Huo Huidan; Zhang Xiangyu; Tian Linhai. Properties of AZ91D Composite Ceramic Coatings Formed with Adding Al2O3 Colloid in MAO Electrolyte. Rare Metal Materials and Engineering, 45(8), pp 2092-2097, 2016-8 [8] 姚晓红; 谢鹏华; 孙永花; 霍慧丹; 张翔宇; 田林海. 微弧氧化电解液中加入Al_2O_3胶体对AZ91D复合陶瓷层性能的影响. 稀有金属材料与工程, (08), pp 2092-2097, 2016-8-15 [9] Wang, Lianbo; Yang, Weiyou; Chong, Haining; Wang, Lin; Gao, Fengmei; Tian, Linhai; Yang, Zuobao. Efficient ultraviolet photodetectors based on TiO2 nanotube arrays with tailored structures. RSC Advances, 5(65), pp 52388-52394, 2015 [10] 续晓霄; 戴姣燕; 符轲; 吴建峰; 田林海; 徐金富.放电等离子烧结氧化锆陶瓷的工艺优化及性能. 金属热处理, (08), pp 154-159, 2015-8-25 [11] 周鹏; 林乃明; 田伟; 姚小飞; 田林海; 唐宾. TC4合金微弧氧化层的耐磨性和耐蚀性. 表面技术, (11), pp 14-20, 2015-11-4 17:22 [12] 杨晓宁; 邓伟林; 黄晓波; 田林海. 高熵合金制备方法进展. 热加工工艺, (22), pp 30-33, 2014 [13] 钱老红; 田林海; 姚晓红; 唐宾. 多孔SnO_2-TiO_2复合膜的制备及其光催化性能. 机械工程材料, (12), pp 54-59, 2014 [14] 姚晓红; 张翔宇; 马永; 范爱兰; 田林海; 唐宾. Ti6Al4V表面等离子Cu/Ni合金化(英文).稀有金属材料与工程, (03), pp 559-562, 2014 [15] Tian, Linhai; Qian, Laohong; Yao, Xiaohong; Li, Xiaoying. Preparation of Sn4+-Doped Titanium Dioxide Photocatalytic Films on 304 Stainless Steel by Duplex Treatment. Journal of Materials Engineering and Performance, 23(5), pp 1790-1798, 2014-5 [16] Yao, Xiaohong; *Zhang, Xiangyu; Wu, Haibo; Tian, Linhai; Ma, Yong; Tang, Bin. Microstructure and antibacterial properties of Cu-doped TiO2 coating on titanium by micro-arc oxidation. Applied Surface Science, 292, pp 944-947, 2014-2-15 [17] Yao Xiaohong; *Zhang Xiangyu; Ma Yong; Fan Ailan; Tian Linhai; Tang Bin. Surface Modification of Ti6Al4V by Plasma Copper and Nickel Alloying Process. Rare Metal Materials and Engineering, 43(3), pp 559-562, 2014-3 [18] Yao Xiaohong; Huo Huidan; Bao Mingdong; *Tian Linhai. Impact fatigue behavior of ZrN/Zr-N/Zr coatings on H13 steel by CFUBMSIP.Journal of Wuhan University of Technology-Materials Science Edition, 29(1), pp 137-142, 2014-2 [19] Yao Xiaohong; Zhang Lin; Gao Wenli; *Tian Linhai. Effect of Aging Treatment on Mechanical and Intergranular Corrosion Properties of 7A85 High Strength Aluminum Alloy. Rare Metal Materials and Engineering, 42(12), pp 2581-2585, 2013-12 [20] 杨晓飞; 田林海; 曹盛; 姚晓红; 唐宾. 纳米TiO_2掺杂对AZ91D镁合金微弧氧化膜形貌及性能的影响.机械工程材料, (10), pp 79, 2013 [21] Zhang, Xiangyu; Hang, Ruiqiang; Wu, Haibo; Huang, Xiaobo; Ma, Yong; Lin, Naiming; Yao, Xiaohong; Tian, Linhai; *Tang, Bin.Synthesis and antibacterial property of Ag-containing TiO2 coatings by combining magnetron sputtering with micro-arc oxidation. Surface and Coatings Technology, 235, pp 748-754, 2013-11-25 [22] 姚晓红; 张林; 高文理; 田林海. 时效状态对7A85高强铝合金力学性能和晶间腐蚀性能的影响. 稀有金属材料与工程, (12), pp 2581-2585, 2013 [23] 韩富银; 王萍; 田林海; 梁伟; 游家学; 钟茜婷. 等通道转角挤压对耐热镁合金AZ61-4Si组织及性能的影响. 稀有金属材料与工程, (07), pp 1497-1501, 2013 [24] *Cao, Sheng; Zheng, Jinju; Zhao, Jialong; Wang, Lin; Gao, Fengmei; Wei, Guodong; Zeng, Ruosheng; Tian, Linhai; Yang, Weiyou. Highly efficient and well-resolved Mn2+ ion emission in MnS/ZnS/CdS quantum dots.JOURNAL OF MATERIALS CHEMISTRY C, 1(14), pp 2540-2547, 2013 [25] *Han Fuyin; Wang Ping; Tian Linhai; Liang Wei; You Jiaxue; Zhong Xiting. Effect of Equal Channel Angular Pressing on Microstructure and Properties of AZ61-4Si Heat-Resistant Magnesium Alloy. Rare Metal Materials and Engineering, 42(7), pp 1497-1501, 2013-7 [26] Yao Xiaohong; *Tian Linhai; Zhang Yang; Ma Yong; Tang Bin. Adhesion and Wear Properties of Cr-N Coatings on Magnesium Alloy by Unbalanced Magnetron Sputtering. Rare Metal Materials and Engineering, 42(3), pp 589-592, 2013-3 [27] *Tian, Linhai; Zhang, Yang; Ma, Yong; Zhu, Xiaodong; Tang, Bin. Effect of Cu content and ion beam bombardment on microstructure and mechanical properties of Cr-Cu-N films. Surface and Coatings Technology, 228, 2013-8-15 [28] 田林海; 张杨; 杨晓飞; 姚晓红.新型环保镁合金微弧氧化复合电解液体系的优化.澳门37000Cm威尼斯学报, (06), pp 646-650, 2012 [29] *Ma Yong; Yu Haifeng; Tian Linhai; Zhang Xiangyu; Tang Bin. Effect of AISI-304 SS Substrate on Ti and Cr Thin Films with Finite Element Simulation. Rare Metal Materials and Engineering, 41, pp 553-556, 2012-9 [30] Tian Linhai; Zhang Yang; Yang Yaojun; Zhu Xiaodong; *Tang Bin. Microstructure and Tribological Behavior of Cr-Cu-N Coatings Deposited by Ion Beam Assisted Magnetron Sputtering. Rare Metal Materials and Engineering, 41, pp 355-358, 2012-2 [31] Zhu Ruihua; *Tian Linhai; Bao Mingdong; Yong, Ma; Bin, Tang. Wear Properties of Plasma Nitrided H13 Steel at Room and Elevated Temperature. Rare Metal Materials and Engineering, 41, pp 203-206, 2012-2 [32] Zhang Xiangyu; *Tang Bin; Fan Ailan; Ma Yong; Tian Linhai. Preparation and Characterization of Plasma Cu Surface Modified Stainless Steel. Journal of Wuhan University of Technology-Materials Science Edition, 27(2), pp 260-264, 2012-4 [33] Tian Linhai; Zhu Ruihua; Yao Xiaohong; Yang Yaojun; *Tang Bin. Fracture behavior of CrN coatings under indentation and dynamic cycle impact. Journal of Wuhan University of Technology-Materials Science Edition, 27(3), pp 411-414, 2012-6 [34] Hang, Ruiqiang; Huang, Xiaobo; Tian, Linhai; He, Zhiyong; *Tang, Bin. Preparation, characterization, corrosion behavior and bioactivity of Ni2O3-doped TiO2 nanotubes on NiTi alloy. Electrochimica Acta, 70, pp 382-393, 2012-5-30 [35] Dong, Y.; Li, X.; Tian, L.; Bell, T.; Sammons, R. L.; Dong, H. Towards long-lasting antibacterial stainless steel surfaces by combining double glow plasma silvering with active screen plasma nitriding. Acta Biomaterialia, 7(1), pp 447-457, 2011-1 [36] 朱瑞华; 田林海; 鲍明东; 马永; 唐宾. H13钢表面不含白亮层的渗氮层制备及其耐磨性能. 机械工程材料, (08), pp 66-69, 2011 [37] *Tian Linhai; Zhu Xiaodong; Tang Bin; Pan Junde; He Jiawen. Fracture Toughness and Repeated Impact Fatigue Properties of Cr-N Hard Coatings. Rare Metal Materials and Engineering, 39, pp 35-38, 2010-6 [38] 张岩; 李晓芳; 田林海; 唐宾. 温度对AZ91D镁合金表面渗镀铝涂层组织结构和性能的影响. 轻合金加工技术, (10), 2010-10-20 [39] 刘二强; 鲍明东; 田林海; 唐宾. 元素成分对磁控溅射TiNi薄膜结构性能的影响及其控制. 电镀与涂饰, (07), 2009-7-15 [40] Yu Chunyan; Tian Linhai; Wei Yinghui; Wang Shebin; Li Tianbao; Xu Bingshe. The effect of substrate bias voltages on impact resistance of CrAlN coatings deposited by modified ion beam enhanced magnetron sputtering. Applied Surface Science, 255(7), pp 4033-4038, 2009-1-15 [41] Yu, Chunyan; Wang, Shebin; Tian, Linhai; Li, Tianbao; Xu, Bingshe. Microstructure and mechanical properties of CrAlN coatings deposited by modified ion beam enhanced magnetron sputtering on AISI H13 steel. Journal of Materials Science, 44(1), pp 300-305, 2009-1 [42] Effect of TiN/CrN Multilayer Coating by Cathodic Arc Deposition on Wear and Corrosion Behaviours of AZ91D Magnesium Alloy [43] Tian, Linhai; Liu, Erqiang; Fan, Ailan; Qin, Lin; Liu, Daoxin; Tang, Bin; Pan, Junde [44] International Materials Research Conference, 2008-6-9 ~ 2008-6-12, pp 870-873, 2009 [45] Microstructure and mechanical properties of Cr–N coatings by ion-beam-assisted magnetron sputtering [46] Linhai Tian, Xiaodong Zhu, Bin Tang, Junde Pan and Jiawen He, [47] Materials Science and Engineering A, 2008, 483–484: 751–754. 二、 授权发明专利 [1] 田林海,姚晓红,张杨,杨晓飞,马永,唐宾.一种镁合金板的微弧氧化法镀膜方法, ZL201210175740.X, 2015. [2] 田林海,钱老红,杨晓飞,姚晓红,林乃明.一种不锈钢表面TiO 2 渗镀层的制备方法, ZL201310285132.9, 2015. [3] 姚晓红,田林海,马永.一种用于甲烷二氧化碳重整制合成气的堇青石基体催化剂及其制备方法, 201110261023.4 [4] 秦林,田林海,范爱兰,姚晓红,武晶晶,唐宾. 金属表面形成Ti-B陶瓷复合材料的方法, ZL 2008 1 0055392.6,2009. |